Key Takeaways
- Today's permanent printing resins are being used for definitive restorations, but long-term clinical data, especially for full-coverage crowns, is still building.
- Printed resin flexes instead of behaving like brittle glass, which changes how you think about prep design, minimum thickness, and chairside adjustment.
- More filler isn't automatically better. Every formulation trades strength against flexibility and other properties.
- Bond printed resin with air abrasion, not etching, then clean thoroughly and prime with a silane or a Bis-GMA–containing primer or adhesive.
- When a printed restoration comes off, look at where the cement stayed. It tells you which side of the bond failed.
Want to go deeper on 3D printed resins? Tune in to the full conversation between Dr. Rolando Nuñez and Dr. Jeff Trembley on Episode 50 of Bonding & Beer.
3D printed restorations get talked about in two very different ways: as the future of restorative dentistry, or as a provisional-grade shortcut that never quite delivered. Both camps are often describing different technology.
So, are 3D printed resins ready for permanent restorations? For a growing range of cases, yes. Current permanent printing resins are made for definitive work, lab studies show them holding up to fatigue testing alongside lithium disilicate (IPS e.max), and clinicians are seating them every day. What's still missing is long-term clinical data, especially for full-coverage crowns.
BISCO has spent 45 years studying how restorative materials bond and behave under load, and printed resins raise those same questions in a new form: how the material flexes, what it takes to bond it, and where its trade-offs sit. Those answers matter more than the hype in either direction.
This article breaks down what changed to make printed resin viable for final restorations, how it behaves differently than porcelain, how to bond it, what clinicians are using it for, and where it still falls short, drawing on Dr. Rolando Nuñez's conversation with Dr. Jeff Trembley on Episode 50 of Bonding & Beer.
From Models to Final Restorations: What Changed?
Dr. Jeff Trembley runs a cosmetic-focused private practice in Nashville, and he's been printing since 2018. For years, that meant models, smile-trial mockups, and prep guides: useful, but nothing he'd leave in a patient's mouth. Early attempts at printed inlays taught hard lessons about cement gap and taper settings, and the materials themselves weren't built for definitive work.
Two things changed: the printers and the resins. Newer systems can handle thicker, more highly filled resins (for Dr. Trembley, the turning point was SprintRay's Midas printer), and each material generation has handled and polished noticeably better than the last. His point to skeptics is simple. If you tried printing a few years ago and walked away, you were judging a different generation of the technology.
“In dentistry, we're limited by materials, but we're also liberated by materials,” he said on the episode.
Why Does Printed Resin Behave So Differently Than Porcelain?
Porcelain is glass. It's strong, but it's rigid and brittle, which is why it needs minimum thicknesses and why a thin veneer can fail all at once. Dr. Trembley compares it to a phone screen: it doesn't matter how strong the glass is. If it flexes, it cracks, and that's why everyone walks around with a case on their phone.
Printed hybrid resin can give a little. Think of how engineers learned to build taller: instead of stacking heavier stone, they used materials that could sway. In one lab study, a printed crown material showed lower flexural strength but greater ductility than lithium disilicate. Bonded 1.2 mm onlays of both materials survived 2 million fatigue cycles without cracks, there was no significant difference in load to failure, and the printed material caused less wear on opposing enamel.1
That flexibility changes how failure tends to look. In Dr. Trembley's experience, a thin printed restoration is more likely to chip than to pop off. On the podcast, he went as far as saying it would never debond, and Dr. Nuñez pushed back right away: what works in one clinician's hands doesn't automatically transfer to every operatory. Asked later whether the chip-instead-of-debond pattern holds up, Dr. Nuñez was direct. It's Dr. Trembley's personal experience and opinion, and “time will tell.”
Dr. Nuñez also raised a fair biomimetic question on air. Enamel is a stiff tissue. When a more flexible material replaces it, how closely does that restoration really mimic the tooth? There isn't a settled answer yet, and it's worth keeping in mind as the evidence grows.
Printed Resin vs. Porcelain at a Glance
What Does This Mean for Tooth Preparation?
Because printed resin doesn't carry porcelain's minimum-thickness requirement in his experience, and can be adjusted to very fine tolerances after it's seated, Dr. Trembley has moved toward additive, minimal-prep and no-prep designs. His framing is memorable: with porcelain, we shape the biology to fit the material. With printed resin, the material wraps around the biology.
In practice, that means bonding restorations in place, then opening embrasures and refining contours chairside, something you can't do to glazed porcelain without losing the surface. He reports no temporaries and most seat appointments done without anesthesia. That's one clinician's workflow rather than a universal outcome, but it shows why the material is pulling some dentists toward more conservative treatment.
Is Stronger Always Better? The Filler Trade-Off
If more filler makes a material stronger, why not pack in as much as possible? Because every formulation is a trade-off. Inorganic filler adds strength and stiffness, while the resin matrix provides the flex. Push the filler too far and you may gain strength but give up the very flexibility that makes printed resin useful.
Dr. Nuñez uses radiopacity to show how this plays out. Adding ytterbium fluoride makes a material more radiopaque, so it shows up more clearly on an X-ray. But BISCO has seen in the lab that adding more of this filler has a detrimental impact on physical properties. Formulators have to find the point where the gain stops being worth the cost. That's why material generations feel so different, and why the highest number on a spec sheet isn't the whole story.
How Do You Bond a 3D Printed Restoration?
Start with the restoration. According to Dr. Nuñez, the intaglio surface should be air-abraded to create mechanical retention, and printed resins should not be etched. The research lines up: in one study of two printed permanent resins, sandblasting produced rougher surfaces and higher bond strengths than hydrofluoric acid etching.2 It's the same principle behind mechanical retention on any bonded surface.
After air abrasion, clean the surface thoroughly and place a primer. Which primer depends on the material. Silane bonds to glass filler, so whether it's worth using depends on the resin's inorganic filler percentage. The other option is a primer or adhesive that contains Bis-GMA, such as All-Bond Universal, which works with the methacrylate resin that makes up most of these materials. This approach applies whichever company made the printer or the resin.
On the tooth side, perform the bonding procedure you prefer. Then match the cement to the restoration: a light-cured resin cement such as Choice 2 is the best option for veneers, and a dual-cured resin cement such as Duo-Link Universal makes sense for everything else. For more on choosing cements for indirect work, see Can a Luting Cement Actually Protect the Tooth After Cementation?
Why Did My Printed Restoration Come Off?
When a printed restoration debonds, Dr. Nuñez's first step is simple: look at where the cement is. If the cement stayed on the restoration, the bond to the tooth failed. If the cement stayed on the tooth, the bond to the restoration failed. That tells you which half of your protocol to adjust.
He hasn't heard a specific, consistent failure pattern from clinicians yet, so treat each case as its own diagnosis rather than assuming a known weak spot.
Debond Diagnosis: Follow the Cement
What Are Clinicians Using Printed Resin For?
In Dr. Trembley's practice, printed resin covers cosmetic anterior cases, inlays, and bonded tabletops. One case stands out: a patient with a deep bite who wanted veneers. Instead of placing upper veneers and letting the lower teeth wear, his team designed the opened bite digitally and bonded printed tabletops from premolar to premolar, without anesthesia.
He also believes printed resin may suit implant restorations better than ceramic, since an implant has no periodontal ligament to absorb force and the material's flex may help. Dr. Nuñez's take is the honest one: that's Dr. Trembley's personal experience and opinion, and only time and data will confirm it.
Where Does Printed Resin Still Fall Short?
The biggest gap is long-term clinical evidence. Even Dr. Trembley, an enthusiastic adopter, doesn't routinely cut off existing crowns to replace them with printed resin, and he hasn't yet seen long-term results for full-coverage crowns. Lab data adds a caution too: in one study, artificial aging lowered the flexural strength of all three printed permanent resins tested.3
There's also a learning curve. Earlier generations were hard to polish, design parameters like cement gap take time to dial in, and results depend heavily on the operator. A workflow that's predictable in one practice won't automatically be predictable in yours on day one.
How Do You Get Started With Printed Restorations?
Dr. Trembley's advice is to start smaller than you think. You don't need to buy every piece of equipment at once; a camera and an intraoral scanner can be enough to begin with an outsourced design-and-print workflow. The one thing he won't budge on is clinical photography. If you're doing cosmetic work, learn it.
The Bottom Line
Printed resin isn't a provisional shortcut anymore, and it isn't a finished story either. The material behaves differently than porcelain, which opens the door to more conservative, adjustable restorations, but success still comes down to the fundamentals: good design, a sound bonding protocol, and the right cement. If you want to sharpen the bonding side, our breakdown of mechanical retention is a natural next read.
Want to go deeper on 3D printed resins? Tune in to the full conversation between Dr. Nuñez and Dr. Trembley on Episode 50 of Bonding & Beer.
Frequently Asked Questions
Can 3D printed resin be used for permanent crowns?
Some printed resins are made for definitive crowns, and lab data is encouraging, but long-term clinical evidence for full-coverage crowns is still limited. Many clinicians currently use printed resin most confidently for veneers, onlays, tabletops, and inlays.
Should you etch a 3D printed restoration before bonding?
No. Printed resins should be air-abraded to create mechanical retention, cleaned thoroughly, and then primed. Research shows air abrasion produces higher bond strength to printed permanent resins than hydrofluoric acid etching.
Do you need silane to bond 3D printed resin?
It depends on the material's inorganic filler percentage. Silane bonds to glass filler, so it may help with more highly filled resins. A primer or adhesive containing Bis-GMA is another option.
What cement should you use for 3D printed restorations?
Bond the tooth with your preferred adhesive procedure. Use a light-cured resin cement for veneers and a dual-cured resin cement for other printed restorations.
How can you tell why a printed restoration debonded?
Look at where the cement is. Cement left on the restoration means the bond to the tooth failed; cement left on the tooth means the bond to the restoration failed.
References
- Bora PV, Lawson NC, Givan DA, Arce C, Roberts H. Enamel wear and fatigue resistance of 3D printed resin compared with lithium disilicate. J Prosthet Dent. 2025. https://doi.org/10.1016/j.prosdent.2024.10.024
- Ersöz B, Aydın N, Ezmek B, Karaoğlanoğlu S, Çal İK. Effect of surface treatments applied to 3D printed permanent resins on shear bond strength. J Clin Exp Dent. 2024. https://doi.org/10.4317/jced.61884
- Korkmaz YN, Buyuk SK, Simsek H. Comparison of the flexural strength of three different aged and nonaged 3D-printed permanent crown resins. Int J Prosthodont. 2024;37(suppl):s203–s207. https://doi.org/10.11607/ijp.8987